other
Blog
Why After Spraying Has Poor Leveling Performance, With Obvious Orange Peel? Aug 03, 2022

Why After Spraying Has Poor Leveling Performance, With Obvious Orange Peel?

1. Coating is too thick or too thin

Solution: Control the coating thickness by adjusting the coating equipment


2. Baking temperature is too low

Solution: Adjust the baking temperature to the correct value


3. The oven heats up too fast, forming a heavy orange peel

Solution: Appropriately slow down the rate of temperature rise, the general workpiece from room temperature to the curing temperature of the time required to control the 4-5 minutes is good


4. Strong reverse ionization

Solution:

A) adjust the static voltage
B) move the gun away from the workpiece
C) check whether the grounding is good


5. Poor quality of the powder coating

Solution: Notify powder suppliers to adjust formulations to improve leveling